- “BCC dual phase refractory superalloy with high phase stability and manufacturing method therefore”
Name of Country in which applied: USA
Persons Registered: E.S. Park, S.J. Kim, J.Y. Kim, H.S. Oh, K.N. Yoon
Application Number (date): USA, US 17/965,103 (Oct. 13 2022)
Registration Number (date): US 11,732,335 B2, (Aug. 22 2023)