Enhanced crack propagation resistance after healing treatment by addition of boron in FeNi-base superalloy

Enhanced crack propagation resistance after healing treatment by addition of boron in FeNi-base superalloy

저자

C.I. Kim, J.Y. Lee, W.T. Kim, E.S. Park, D.H. Kim

저널 정보

Materials Science and Engineering: A, 903 (2024) 146664.

출간연도

2024

C.I. Kim, J.Y. Lee, W.T. Kim, E.S. Park, D.H. Kim, “Enhanced crack propagation resistance after healing treatment by addition of boron in FeNi-base superalloy”, Materials Science and Engineering: A, 903 (2024) 146664.